MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ITW Irathane Futura® IRABOND RU80 Primer
Categories: Polymer; Adhesive; Thermoset

Material Notes: A single component brush applied primer developed for use when coating or repairing cured rubber substrates.

RECOMMENDED APPLICATIONS: Suitable primer when repairing cured rubber in conjunction UU55 or UU52 and Irathane or Aqualine system coat.

FEATURES• Rapid cure • Enhances bonding to rubbers for a number of Irathane systems.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 2.0 %2.0 %± 1%. By volume
 
Thermal PropertiesMetricEnglishComments
Flash Point -4.00 °C24.8 °F
 
Processing PropertiesMetricEnglishComments
Pot Life  <= 120 min
@Temperature 30.0 °C
<= 120 min
@Temperature 86.0 °F
 <= 180 min
@Temperature 20.0 °C
<= 180 min
@Temperature 68.0 °F
 <= 240 min
@Temperature 10.0 °C
<= 240 min
@Temperature 50.0 °F
Shelf Life 12.0 Month
@Temperature 22.0 °C
12.0 Month
@Temperature 71.6 °F
In original unopened container in dry environment.
 
Descriptive Properties
ColorColorless
Coverage8-10m²/L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWI9242 / 239751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.