MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TechnoCompound TechnoFin PP LR Polypropylene, 23% Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Information provided by TechnoCompound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Melt Flow 5.0 g/10 min
@Load 0.00216 kg,
Temperature 230 °C
5.0 g/10 min
@Load 0.00476 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 41.0 MPa
@Load 36.5 kg
5950 psi
@Load 80.5 lb
ISO 2039-1
Tensile Strength at Break 22.0 MPa3190 psi5 mm/min; ISO 527
Tensile Strength, Yield 22.0 MPa3190 psi50 mm/min; ISO 527
Elongation at Break 9.0 %9.0 %5 mm/min; ISO 527
Elongation at Yield 5.5 %5.5 %50 mm/min; ISO 527
Tensile Modulus 1.20 GPa174 ksi1 mm/min; ISO 527
Flexural Strength 28.04 MPa4067 psi2 mm/min; ISO 178
Flexural Modulus 1.176 GPa170.6 ksi2 mm/min; ISO 178
Charpy Impact Unnotched  0.819 J/cm²
@Temperature -30.0 °C
3.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  0.421 J/cm²
@Temperature -30.0 °C
2.00 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 0.819 J/cm²
@Temperature 23.0 °C
3.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 ohm10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C183 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTECHNO013 / 306375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.