SABIC® STAMAX 60YM240E is a 60% long glass fiber reinforced low emission concentrate and specially developed for dilution with low emission SABIC® PP homopolymer. The glass fibres are chemically coupled to the PP matrix, resulting in high stiffness and strength
IMDS ID: 16501821Information provided by SABIC |