MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott LF5G19 597399.330, Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.30 g/cc0.119 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 3.43.4
Alkali Class, AR 2.22.2
Stain Resistance Class, FR 2.02.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 410410HK (0.1/20)
Modulus of Elasticity 56.0 GPa8120 ksi
Poissons Ratio 0.2420.242
Shear Modulus 22.5 GPa3260 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.7 µm/m-°C
@Temperature -30.0 - 70.0 °C
5.94 µin/in-°F
@Temperature -22.0 - 158 °F
 11.4 µm/m-°C
@Temperature 20.0 - 300 °C
6.33 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.580 J/g-°C0.139 BTU/lb-°F
Thermal Conductivity 0.750 W/m-K5.20 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 474 °C885 °F
Softening Point 606 °C1120 °Fviscosity of 107.6 cP
Annealing Point 462 °C864 °Fviscosity of 1013 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.564
@Wavelength 2325.4 nm
1.564
@Wavelength 2325.4 nm
 1.568
@Wavelength 1970.1 nm
1.568
@Wavelength 1970.1 nm
 1.574
@Wavelength 1529.6 nm
1.574
@Wavelength 1529.6 nm
 1.58
@Wavelength 1060 nm
1.58
@Wavelength 1060 nm
 1.581
@Wavelength 1014 nm
1.581
@Wavelength 1014 nm
 1.584
@Wavelength 852.1 nm
1.584
@Wavelength 852.1 nm
 1.589
@Wavelength 706.5 nm
1.589
@Wavelength 706.5 nm
 1.592
@Wavelength 656.3 nm
1.592
@Wavelength 656.3 nm
 1.592
@Wavelength 613.8 nm
1.592
@Wavelength 613.8 nm
 1.59349
@Wavelength 632.8 nm
1.59349
@Wavelength 632.8 nm
 1.596
@Wavelength 5289.3 nm
1.596
@Wavelength 5289.3 nm
 1.596
@Wavelength 587.6 nm
1.596
@Wavelength 587.6 nm
 1.60
@Wavelength 546.1 nm
1.60
@Wavelength 546.1 nm
 1.607
@Wavelength 486.1 nm
1.607
@Wavelength 486.1 nm
 1.60799
@Wavelength 480 nm
1.60799
@Wavelength 480 nm
 1.615
@Wavelength 435.8 nm
1.615
@Wavelength 435.8 nm
 1.623
@Wavelength 404.7 nm
1.623
@Wavelength 404.7 nm
Abbe Number 39.639.6ve
 39.8939.89vd
Optical Dispersion 0.0149540.014954nf - nc
 0.0151530.015153nf' - nc'
Transmission, Visible  35 %
@Thickness 25.0 mm,
Wavelength 420 nm
35 %
@Thickness 0.984 in,
Wavelength 420 nm
 61.2 %
@Thickness 25.0 mm,
Wavelength 436 nm
61.2 %
@Thickness 0.984 in,
Wavelength 436 nm
 65.7 %
@Thickness 10.0 mm,
Wavelength 420 nm
65.7 %
@Thickness 0.394 in,
Wavelength 420 nm
 82.2 %
@Thickness 10.0 mm,
Wavelength 436 nm
82.2 %
@Thickness 0.394 in,
Wavelength 436 nm
 83.2 %
@Thickness 25.0 mm,
Wavelength 460 nm
83.2 %
@Thickness 0.984 in,
Wavelength 460 nm
 92.9 %
@Thickness 10.0 mm,
Wavelength 460 nm
92.9 %
@Thickness 0.394 in,
Wavelength 460 nm
 93.4 %
@Thickness 25.0 mm,
Wavelength 500 nm
93.4 %
@Thickness 0.984 in,
Wavelength 500 nm
 96.6 %
@Thickness 25.0 mm,
Wavelength 546 nm
96.6 %
@Thickness 0.984 in,
Wavelength 546 nm
 97.3 %
@Thickness 10.0 mm,
Wavelength 500 nm
97.3 %
@Thickness 0.394 in,
Wavelength 500 nm
 97.7 %
@Thickness 25.0 mm,
Wavelength 580 nm
97.7 %
@Thickness 0.984 in,
Wavelength 580 nm
 98.3 %
@Thickness 25.0 mm,
Wavelength 620 nm
98.3 %
@Thickness 0.984 in,
Wavelength 620 nm
 98.6 %
@Thickness 10.0 mm,
Wavelength 546 nm
98.6 %
@Thickness 0.394 in,
Wavelength 546 nm
 98.7 %
@Thickness 25.0 mm,
Wavelength 660 nm
98.7 %
@Thickness 0.984 in,
Wavelength 660 nm
 99.1 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.1 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.3 %
@Thickness 25.0 mm,
Wavelength 700 nm
99.3 %
@Thickness 0.984 in,
Wavelength 700 nm
 99.3 %
@Thickness 10.0 mm,
Wavelength 620 nm
99.3 %
@Thickness 0.394 in,
Wavelength 620 nm
 99.5 %
@Thickness 10.0 mm,
Wavelength 660 nm
99.5 %
@Thickness 0.394 in,
Wavelength 660 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.7 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  20 %
@Thickness 25.0 mm,
Wavelength 2500 nm
20 %
@Thickness 0.984 in,
Wavelength 2500 nm
 31.6 %
@Thickness 25.0 mm,
Wavelength 2325 nm
31.6 %
@Thickness 0.984 in,
Wavelength 2325 nm
 52.5 %
@Thickness 10.0 mm,
Wavelength 2500 nm
52.5 %
@Thickness 0.394 in,
Wavelength 2500 nm
 63.1 %
@Thickness 10.0 mm,
Wavelength 2325 nm
63.1 %
@Thickness 0.394 in,
Wavelength 2325 nm
 70.7 %
@Thickness 25.0 mm,
Wavelength 1970 nm
70.7 %
@Thickness 0.984 in,
Wavelength 1970 nm
 87 %
@Thickness 10.0 mm,
Wavelength 1970 nm
87 %
@Thickness 0.394 in,
Wavelength 1970 nm
 97.9 %
@Thickness 25.0 mm,
Wavelength 1530 nm
97.9 %
@Thickness 0.984 in,
Wavelength 1530 nm
 99.2 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.2 %
@Thickness 0.394 in,
Wavelength 1530 nm
 99.8 %
@Thickness 25.0 mm,
Wavelength 1060 nm
99.8 %
@Thickness 0.984 in,
Wavelength 1060 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 1060 nm
99.9 %
@Thickness 0.394 in,
Wavelength 1060 nm
UV Transmittance  4.0 %
@Thickness 25.0 mm,
Wavelength 400 nm
4.0 %
@Thickness 0.984 in,
Wavelength 400 nm
 9.0 %
@Thickness 10.0 mm,
Wavelength 390 nm
9.0 %
@Thickness 0.394 in,
Wavelength 390 nm
 9.0 %
@Thickness 25.0 mm,
Wavelength 405 nm
9.0 %
@Thickness 0.984 in,
Wavelength 405 nm
 27.6 %
@Thickness 10.0 mm,
Wavelength 400 nm
27.6 %
@Thickness 0.394 in,
Wavelength 400 nm
 38.2 %
@Thickness 10.0 mm,
Wavelength 405 nm
38.2 %
@Thickness 0.394 in,
Wavelength 405 nm
 
Descriptive Properties
Climatic resistance3
Grindability2ISO 12844
Phosphate resistance3
Stress optical coefficient2.8[10-6mm2/N]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ohara S-PHM52 Optical Glass
Schott LG-680 Silicate Laser Glass
Schott BG3 Band Pass Filter
Ohara L-TIM28 Low Tg Optical Glass
AISI E4340 Steel, oil quenched 845°C, 650°C (1200°F) temper

CSGT9865 / 183118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.