Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processing Key Features and Benefits: - Meets MIL-R-7575 requirements
- 160°F max service temperature
- Good electrical properties
- Low cure temp (190°F) for easy processing
Applications/Qualifications: - Aircraft window frames
- Industrial Parts
- Automotive applications
Information provided by Park Electrochemical Corp. |