DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with
improved surface tack that produces superior grip qualities. DGR 6040NCEHT will bond to olefinics, and is easily colored. DuraGrip® is not hygroscopic and under normal conditions does
not require drying. Information provided by Advanced Polymer Alloys Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014. |