  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
Categories: Metal; Ferrous Metal; Stainless Steel; Superalloy; Iron Base

Material Notes: Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at high temperatures. Specific uses include jet engine nacelles, parts, and fasteners. Allegheny Ludlum Altemp A286 alloy is a heat and corrosion resistant austenitic iron-base material which can be age hardened o a high strength level. The alloy is also used for low temperature applications requiring a ductile, non-magnetic high strength material at temperatures ranging from above room temperature down to -196 degrees Celsius. The alloy may be used for moderate corrosion applications in aqueous solutions. This alloy can be produced by AOD refining or vacuum induction melting. Vacuum arc or electroslag remelting procedures may be used to further refine the material.

Information provided by Allegheny Ludlum

Key Words: AMS 5525; AMS 5858 (Welding Quality)
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.92 g/ccSolution Treated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85Typical Annealed
Tensile Strength, Ultimate 620 MPaSolution Treated (Typical)
Tensile Strength, Yield 275 MPaSolution Treated (Typical)
Elongation at Break 40 %Solution Treated (Typical)
Modulus of Elasticity 201 GPaDynamic
Poissons Ratio 0.30
Shear Modulus 77.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000910 ohm-cm
Magnetic Permeability 1.01Solution Treated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 20.0 - 93.0 °C
 17.0 µm/m-°C
@Temperature 20.0 - 315 °C
 17.6 µm/m-°C
@Temperature 20.0 - 538 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 15.1 W/m-K
@Temperature 150 °C
Melting Point 1370 - 1430 °C
Solidus 1370 °C
Liquidus 1430 °C
Maximum Service Temperature, Air 816 °CContinuous service
 982 °CIntermittent
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.15 %
Boron, B 0.0060 %
Carbon, C 0.040 %
Chromium, Cr 14.5 %
Iron, Fe 56 %as balance
Manganese, Mn 0.20 %
Molybdenum, Mo 1.25 %
Nickel, Ni 25 %
Phosphorus, P 0.015 %
Silicon, Si 0.20 %
Sulfur, S 0.0020 %
Titanium, Ti 2.1 %
Vanadium, V 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
660 Stainless Steel (A286) short time tensile test
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
A286 IRON BASED 15Cr-26Ni-1.3Mo-2.1Ti-0.3V SUPERALLOY FORGINGS FOR GAS TURBINE DISCS
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 425°C (800°F)
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy (UNS S66286)

NLA286 / 17965

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.