MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent characteristics of polycarbonate resin

Applications:

  • Mechanical, electric and electronic components that need abrasion and friction resistance.
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.36 g/ccISO 1183
    Moisture Absorption 0.140 %
    @Temperature 23.0 °C,
    Time 86400 sec
    ISO 62
    Linear Mold Shrinkage, Flow 0.00020 - 0.0020 cm/cm
    @Thickness 4.00 mm
    Teijin method
    Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
    @Thickness 4.00 mm
    Teijin method
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 120 MPaISO 527-2/5
    Elongation at Break 1.5 %ISO 527-2/5
    Tensile Modulus 13600 MPaISO 527-2/1
    Flexural Strength 170 MPa2.0 mm/min; ISO 178
    Flexural Modulus 12000 MPa2.0 mm/min; ISO 178
    Charpy Impact Unnotched 25.0 kJ/m²ISO 179
    Charpy Impact, Notched 7.00 kJ/m²ISO 179
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 10 - 1000 ohm-cmIEC 60093
    Surface Resistance 1.0 - 100 ohmIEC 60093
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-2
    CTE, linear, Transverse to Flow 60.0 µm/m-°CISO 11359-2
    Deflection Temperature at 0.46 MPa (66 psi) 150 °Cunannealed; ISO 75-2/B
    Deflection Temperature at 1.8 MPa (264 psi) 147 °Cunannealed; ISO 75-2/A
    Vicat Softening Point 152 °CISO 306/B50
    UL RTI, Electrical 80.0 °C
    @Thickness 1.50 mm
    UL 746
    UL RTI, Mechanical with Impact 80.0 °C
    @Thickness 1.50 mm
    UL 746
    UL RTI, Mechanical without Impact 80.0 °C
    @Thickness 1.50 mm
    UL 746
    Flammability, UL94 V-2
    @Thickness 0.750 mm
     V-1
    @Thickness 1.50 mm

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Teijin Technora® Aramid Fiber
    Teijin Panlite® MN-4805Z Transparent Flame Retardant Polycarbonate
    DuPont Teijin Films Melinex® ST730 Polyester Film
    Teijin Panlite® AM-8030 Polycarbonate + Polyester Alloy
    DuPont™ Kevlar® 49 Aramid Fiber

    PTEIJ38 / 69727

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.