MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyplastic Compounds Armlen® PP GF 10-2HS Polypropylene, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: A 10% glass fiber, light-stabilized polypropylene. This material displays high mechanical and thermal properties. Designed for manufacture of railway dowels, may be applied as a substitution of metals, thermosetting polymers and other thermoplastics in construction, specialty and general items. Available in natural and black colors.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm0.0070 - 0.010 in/inISO 294-4
Melt Flow 6.8 g/10 min
@Load 2.16 kg,
Temperature 250 °C
6.8 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.0 MPa7830 psiISO 527-1
Elongation at Break 5.6 %5.6 %ISO 527-1
Flexural Strength 70.0 MPa10200 psiat maximum load; ISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Charpy Impact Unnotched  3.80 J/cm²
@Temperature 23.0 °C
18.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1
 4.00 J/cm²
@Temperature -50.0 °C
19.0 ft-lb/in²
@Temperature -58.0 °F
ISO 179-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 °C324 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °F
Mold Temperature 60.0 °C140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC042 / 307114

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.