MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ PFA 6900GZ Perfluoroalkoxy Fluorothermoplastic Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Dyneon PFA 6900GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a melt-processable copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magnitude lower than PTFE. Outstanding advantages associated with PTFE are:
  • excellent chemical resistance
  • wide service temperature range
  • non-stick properties
  • outstanding soil-and-dirt repellency
  • extremely high weathering resistance
  • nonflammable
  • excellent dielectric properties

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D792
Density 1.43 g/cc0.0517 lb/in³of dispersion; ASTM D1298
Solids Content 50 %50 %ASTM D4441
Particle Size 0.235 µm0.235 µm
pH <= 7.0<= 7.0ASTM E70
Melt Index of Compound 15 g/10 min
@Load 5.00 kg,
Temperature 372 °C
15 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FASTM D4591
 
Descriptive Properties
Surface Active Ingredientsnon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDYNE019 / 34827

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.