MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese FORTRON® 4332D4 Mineral and Glass Reinforced Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Description: Fortron 4332D4 offers a unique balance of properties based on a high mineral and glass reinforced composition, complementing our other 6165 product offerings. The heat resistance under load bearing conditions is excellent for this product. As with all Fortron grades this product is inherently flame-retardant. Applications include electronic and industrial components.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc0.0704 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi5 mm/min; ISO 527-2/1A
Elongation at Break 1.0 %1.0 %5 mm/min; ISO 527-2/1A
Tensile Modulus 21.5 GPa3120 ksi1 mm/min; ISO 527-2/1A
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 21.0 GPa3050 ksiISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 220 °C428 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 340 °C590 - 644 °F
Mold Temperature 135 - 160 °C275 - 320 °F
Drying Temperature 135 °C275 °F
Dry Time 3 - 4 hour3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Celanese FORTRON MT9120L4 PPS, 20% Medical Technology
Celanese FORTRON MT9140L4 PPS, 40% Medical Technology
Celanese FORTRON MT9140L6 PPS, 40% Medical Technology

PHCW52 / 45993

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.