MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: ENR 7086.01 is an ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially available polyolefin elastomers. It is ideally suited for use alone or as an additive to enhance processing in blow molding, extrusion and thermoforming applications where high levels of shear thinning and high melt strength may be required.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.901 g/ccASTM D792
Viscosity 2.00e+6 cP
@Shear Rate 100 1/s,
Temperature 190 °C
100 rad/sec; ARES Rheometer
 6.50e+6 cP
@Shear Rate 10 1/s,
Temperature 190 °C
10 rad/sec; ARES Rheometer
 1.50e+7 cP
@Shear Rate 1.58 1/s,
Temperature 190 °C
1.58 rad/sec; ARES Rheometer
 5.00e+7 cP
@Shear Rate 0.1 1/s,
Temperature 190 °C
0.1 rad/sec; ARES Rheometer
Mooney Viscosity 26
@Temperature 125 °C
ML 1 + 4; ASTM D1646
Melt Index of Compound <= 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 3.6 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
Crystallinity 28.2 %25°C; DuPont Test
 28.8 %
@Temperature -40.0 °C
Total; DuPont Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8810 sec; ASTM D2240
Tensile Strength, Ultimate 20.0 MPa508 mm/min; ASTM D638
Elongation at Break 625 %508 mm/min; ASTM D638
2% Secant Modulus 0.0679 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 93.0 °CDSC, 10°C/min (peak); DuPont Test
Crystallization Temperature 78.0 °CDSC, 10°C/min (peak); DuPont Test
Glass Transition Temp, Tg -35.0 °CDSC, 10°C/min (inf); DuPont Test
 
Descriptive Properties
Molecular Weight DistributionMediumGPC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Dow Engage® 8540 Polyolefin Elastomer
Dow Engage® 8842 Polyolefin Elastomer
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Dow Engage® 8150 Polyolefin Elastomer

PDVE47 / 34108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.