MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound DC0041PR Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DC0041PR compound is based on Polycarbonate (PC) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive, Non-Brominated, Non-Chlorinated Flame Retardant, PCR content up to 30%.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Light-weight Structural,Enhanced Ductility,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Moisture Absorption 0.0500 %0.0500 %Injection Molding
Linear Mold Shrinkage, Flow 0.00080 cm/cm0.00080 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0033 cm/cm0.0033 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psi5 mm/min; ASTM D638
Elongation at Break 1.1 %1.1 %5 mm/min; ASTM D638
Tensile Modulus 19.0 GPa2760 ksi5 mm/min; ASTM D638
Flexural Strength 200 MPa29000 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 17.5 GPa2540 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 55.0 J40.6 ft-lbASTM D256
Izod Impact, Unnotched 4.00 J/cm7.49 ft-lb/inASTM D4812
Dart Drop, Total Energy 9.00 J6.64 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
@Thickness 3.20 mm
187 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 275 - 310 °C527 - 590 °FInjection Molding
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 70.0 °C158 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 63 rpm30 - 63 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81495 / 289442

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.