MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wynca WynPh ® FR800 Halophosphate-free Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Good circulability and no need for any enhancers (e.g. antimony oxide) compared to bromine flame retardants.
  • Low volatility and thermal stability manifested in the production process of most engineering thermoplastic resins.
  • Superior hydrolysis resistance, small mobility and less volatile loss. It can improve the thermal aging performance, increase the thermal deformation temperature, and its excellent fluidity is conducive to the production of thin-walled molds while reducing the burning.
Application and Suggestion:FR800 is particularly suitable for engineering resin alloy, including PC/ABS and PPO-PPE / HIPS for electrical and electronic accessories. According to fire safety standards, FR800 basically used about 8 to 18 phr, which can retain more than 95% in objects at 280?. FR800 can improve melting performance of engineering plastics products, that is suitable as flame retardant for PVC, cellulose resin, synthetic rubber, epoxy resin, etc.

Information provided by Wynca Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.27 g/cc0.0452 - 0.0459 lb/in³
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 8.5 - 9.3 %8.5 - 9.3 %
 
Descriptive Properties
AppearanceColorless / light yellow clear liquid
Content<1.0%TPP
 <500 ppmPhenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWYNCA090 / 320648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.