MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem AKROFAX™ 57 WHITE
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrofax 57 White is a white, medium-hard, vulcanized vegetable oil, made from pure rapeseed oil and mineral stabilizers. It is commonly used in erasers and other white or light colored applications. The sulfur monochloride used to cure the vegetable oil will acidify rubber cures. To overcome the slowing of a cure we recommend adding 3-4 phr of MgO and/or 0.25-0.4phr of a guanidine (DPG or DOTG) to recover cure rate.

Function:

  • Capacity for absorbing large amounts of mineral oils and other liquid plasticizer on mill and banbury.
  • To speed the incorporation of fillers and to increase milling efficiency.
  • To reduce migration of oils and plasticizers to the surface in low durometer stocks.
  • To provide a non-thermoplastic structure in uncured compounds which strengthens extruded sections and minimizes distortions in open steam cures.
  • Ability to flow or promote flow under mechanical pressure.
  • To provide a unique surface finish and supple feel to vulcanized rubber goods.
  • To improve ozone resistance of the rubber compounds.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/cc
Ash 39 - 43 %
 
Descriptive Properties
Appearancecrumb
Content<0.30%Free Sulfur
 0.15Mineral Oil
 15-23%N-hexane Extract

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH618 / 315536

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.