MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Chesterton 763 Rust Transformer®
Categories: Fluid

Material Notes: Description: Chesterton® 763 Rust Transformer® is a mild, natural acid based product which electrochemically transforms rust into a corrosion inhibiting protective film. It is the labor saving way to prepare metals prior to painting. As an alternative to sandblasting, the product provides convenience, low cost, and few health or safety hazards. Flash rusting is eliminated as the thin film formed protects surfaces prior to further coating. Unlike strong acid preparations sometimes used to prepare metals, damage to surfaces and embrittlement is never a problem with 763 Rust Transformer. The product gently but effectively converts surfaces into a receptive base coat for the application of a primer and topcoat.

Features:

  • Easy to apply
  • No sandblasting
  • Forms protective film
  • Cleans up with water
  • No strong acids
  • No elaborate application equipment
  • Biodegradable
  • Safer for workers

Applications: Transforms rust into a corrosion inhibiting coating on storage tanks, auto or truck bodies, heavy equipment, bridges, transmission line towers, ships, piers, structural steel, marine and construction sites, anywhere rust is destroying metal. Quickly and easily provides a good surface for the application of Chesterton® 758 Lead Free Primer.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
pH 1.2
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air 10.0 °C50% relative humidity
 
Descriptive Properties
AppearanceTransparent, Brown
Coverage19.6 m2/l
FormLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTCHS117 / 138229

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.