MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess MF 7980 Milled Fiber
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: LANXESS Glass Fiber MF 7980* is suitable for a wide range of applications where the reinforcing properties of glass fibers are needed in combination with small initial fiber length, no surface treatment and excellent flowability. For example, MF 7980 is excellent for reinforcing integral skin polyurethane foams by the RRIM method (RRIM = Reinforced Reaction Injection Molding). Milled fiber is normally stirred into the polyol during processing, but may also be added to the isocyanites.

MF 7980 consists of individual filaments of different lengths; Small average fiber length of 190 µm nominally. No treatment/sizing; Also suitable for the reinforcement of thermoplastics (particularly polycarbonates). Adding MF 7980 improves, among other things, heat resistance, stiff-ness, strength and dimensional stability and Excellent flowability

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Water Absorption <= 0.050 %<= 0.050 %
 
Descriptive Properties
Specifications14 µmFiber Diameter
 190 mmAv. Fiber Length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8663 / 209056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.