MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Quaker Quintolubric® 888-68 Fire Resistant HFD-U Hydraulic Fluid
Categories: Fluid

Material Notes: Benefits:
  • Global formulation
  • Excellent shear stability
  • Best-in-class oxidation stability
  • Environmentally friendly
Applications: QUINTOLUBRIC® 888-68 was designed to replace anti-wear, mineral oil-based hydraulic fluids used in applications where fire hazards exist. QUINTOLUBRIC® 888-68 can also be used in environmentally sensitive hydraulic applications without compromising the overall hydraulic system operations. This fluid does not contain water, mineral oil, or phosphate ester, and is based on high-quality, synthetic, organic esters and carefully selected additives to achieve excellent hydraulic fluid performance. QUINTOLUBRIC® 888-68 offers the lubrication level of premium, antiwear hydraulic oils, and can be used with hydraulic components from all major manufacturers.

Information provided by Quaker

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc
@Temperature 15.0 °C
0.0332 lb/in³
@Temperature 59.0 °F
ASTM D1298
Viscosity Measurement 185185Index; ASTM D2270
Kinematic Viscosity 135 cSt135 cStASTM D445
Viscosity Measure 554 cSt
@Temperature 0.000 °C
554 cSt
@Temperature 32.0 °F
Kinematic; ASTM D445
Kinematic Viscosity at 40°C (104°F) 68 cSt68 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 12.5 cSt12.5 cStASTM D445
Vapor Pressure  4.27e-9 bar
@Temperature 20.0 °C
0.00000320 torr
@Temperature 68.0 °F
02551
 1.00e-8 bar
@Temperature 66.0 °C
0.00000750 torr
@Temperature 151 °F
02551
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2.02.0[mg KOH/g}; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Bulk Modulus 12.9 GPa
@Pressure 20.7 MPa
1870 ksi
@Pressure 3000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 30000 V30000 VASTM D887
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C3.33 µin/in-°FASTM D1903
Specific Heat Capacity 2.05 J/g-°C0.490 BTU/lb-°FASTM D2766
Thermal Conductivity 0.167 W/m-K
@Temperature 19.0 °C
1.16 BTU-in/hr-ft²-°F
@Temperature 66.2 °F
ASTM D2717
Pour Point <= -30.0 °C<= -22.0 °FASTM D97
Flash Point 304 °C579 °FASTM D92
Ignition Temperature >= 400 °C>= 752 °FAutoignition; DIN 51794
 >= 450 °C>= 842 °FHot Manifold; ISO 20823
 
Descriptive Properties
Air Release7 minASTM D3427
AppearanceYellow to amber fluid
Dry TOST800 hrsASTM D943
Fire Point360°CASTM D92
Foam Test50-0 ml-ml@ 25°C, Sequence I, ASTM D892
Gear Lubrication>12 FZG load stageDIN 51354-2
Pump Test<5 mg wearASTM D2282
Water Separability42-38-0 ml-ml-ml30 min, ASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WQUAK008 / 184994

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.