MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dow™ 751A LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description:
  • A high additive film resin for general packaging applications
  • For cast film extrusion
  • A fast blooming resin for high speed bag conversion
Complies with: US FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objection (with Limitations); EU, No 10/2011; Japan Hygienic Olefin and Styrene Plastics Association. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: 2900 ppm; Processing Aid: No; Slip: 2640 ppm

Agency Ratings: FDA 21 CFR 177.1520©2.1; Canadian HPFB No Objection; EU, No 10/2011; JHOSPA

Form: Pellets

Processing Method: Blown Film; Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D792
Melt Flow 6.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 2900 ppm
Slip Level 2640 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 2010 psi
@Thickness 0.0203 mm
ASTM D882
Film Tensile Strength at Yield, TD 1660 psi
@Thickness 0.0203 mm
ASTM D882
Film Elongation at Break, MD 150 %
@Thickness 0.0203 mm
ASTM D882
Film Elongation at Break, TD 440 %
@Thickness 0.0203 mm
ASTM D882
Elmendorf Tear Strength MD 200 g
@Thickness 0.0203 mm
ASTM D1922
Elmendorf Tear Strength TD 100 g
@Thickness 0.0203 mm
ASTM D1922
Dart Drop Test 25.0 g
@Thickness 0.0203 mm
ASTM D1709A
Film Tensile Strength at Break, MD 4700 psi
@Thickness 0.0203 mm
ASTM D882
Film Tensile Strength at Break, TD 1850 psi
@Thickness 0.0203 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 235 °F
Vicat Softening Point 205 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.4 %
@Thickness 0.0203 mm
ASTM D1003
Gloss 80 %
@Thickness 0.0203 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 449 °FScrew A, B, C, D
 450 °FScrew E
 
Descriptive Properties
Film Puncture Resistance11 ft-lb/in32.0 mil
Film Toughness1140 ft-lb/in3TD, 1.0 mil, ASTM D882
 951 ft-lb/in3MD, 1.0 mil, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF475 / 311168

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.