MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Addovate® WM PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Dispersant and emulsifier for the production of polyester based flexible slabstock foam.

Product information: Addovate WM is an emulsifier for water, paraffin oil and water-insoluble catalysts (e.g. Addocat DB) in polyester-polyols with OH-value of approx. 60 mg KOH/g. This emulsifier is used for the production of polyester slabstock foam with TDI 65. Addovate WM is used in combination with Addovate SM and if necessary Addovate LM (prevents core discoloration). In general 1.0 - 2.0 p.b.w. of Addovate WM should be added to 100 p.b.w. polyester polyol. Over-dosage (> 4.0 p.b.w.) of Addovate WM will result in a deterioration of the compression hardness. Under-dosage of Addovate WM leads to a badly homogenized catalyst mixture which results in severe damages to the cell structure. Should a silicone stabilizer be processed which emulsifies Addocat DB not sufficiently, it is recommended to add a sufficient amount of Addovate WM (approx. 0.5 - 1.0 p.b.w.).

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Viscosity 850 cP850 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.50<= 0.50[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 5.00 °C41.0 °FFreezing Point
Boiling Point 180 °C356 °FInitial
Flash Point 295 °C563 °FDIN ISO 2592
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 10.0 - 30.0 °C
12.0 Month
@Temperature 50.0 - 86.0 °F
 
Descriptive Properties
Appearanceyellowish brown to brown liquid
Hydroxyl value60-80 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8233 / 208626

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.