MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow ENGAGE™ POE 58710 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ENGAGE™ POE 58710 Polyolefin Elastomer is an ethylene-octene copolymer that has good flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer applications. POE 58710 provides desired impact properties in blends with PP and PE. It provides high filler loading capability and good peroxide cure capability. When cross-linked by peroxide, silane, or irradiation, it gives good heat aging, compression set, and weather resistance properties, and may be used to produce high performance electrical insulation.
Main Characteristics:
  • Pellet form
  • Excellent flow characteristics
  • Improved impact in polypropylene and polyethylene
  • High filler loading
  • Peroxide, silane, and radiation curable
  • Exceptional heat aging, compression set, and weather resistance when cured
Applications:
  • General purpose thermoplastic elastomers
  • Wire and cable
  • Impact modification
Availability: Asia Pacific; Europe: Latin America; North America

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.872 g/cc0.0315 lb/in³ASTM D792
Mooney Viscosity 24
@Temperature 121 °C
24
@Temperature 250 °F
ML1+4; ASTM D1646
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73
@Time 1.00 sec
73
@Time 0.000278 hour
Compression Molded; ASTM D2240
Hardness, Shore D 22
@Time 1.00 sec
22
@Time 0.000278 hour
Compression Molded; ASTM D2240
Tensile Strength at Break 9.79 MPa1420 psiCompression Molded, 20 in/min; ASTM D638
Elongation at Break 1420 %1420 %Compression Molded, 20 in/min; ASTM D638
Tensile Modulus 0.00290 GPa0.421 ksi100% Secant, 20 in/min, Compression Molded; ASTM D638
Flexural Modulus 0.0131 GPa1.90 ksi1% Secant, Compression Molded; ASTM D790
 0.0143 GPa2.07 ksi2% Secant, Compression Molded; ASTM D790
Tear Strength 40.0 kN/m228 pliDie C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 °C140 °F
Crystallization Temperature 45.0 °C113 °FPeak
Vicat Softening Point 45.0 °C113 °FASTM D1525
Glass Transition Temp, Tg -52.0 °C-61.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF531 / 311224

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.