MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Wacker Silpuran® 4200 Silicone Adhesive
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: SILPURAN® 4200 is a non-slump to self-leveling silicone rubber formulation, curing at room temperature under the influence of atmospheric moisture to a silicone elastomer with good mechanical properties.

Properties : SILPURAN® 4200 meets selected test requirements of ISO 10993 and United States Pharmacopeia (USP) Class VI.

Special features:

  • acetic acid-curing system
  • non-slump to self-leveling
  • fast curing
  • excellent primerless adhesion to many substrates
  • biocompatible
Application: One-component adhesive, in particular for medical applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccuncured; DIN 53217
 1.10 g/cccured; DIN EN ISO 1183-1/ISO 2781
Viscosity 300000 cPdynamic; DIN EN ISO 3219
 140000 cP
@Shear Rate 100 1/s
DIN EN ISO 3219
 200000 cP
@Shear Rate 10.0 1/s
DIN EN ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35DIN 53505/ISO 868
Tensile Strength at Break 5.50 MPaDIN 53505 S1/ISO 868
Elongation at Break 300 %DIN 53504 S1/ISO 37
Tear Strength 10.0 kN/mASTM D624
 
Processing PropertiesOriginal ValueComments
Cure Time 336 hour
@Treatment Temp. 23.0 °C
2mm, 50% RH
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Colortranslucentcured
 translucentuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 4305/50 Silicone Rubber
Wacker Elastosil® R 420/50 Silicone Rubber

PWACK9483 / 205012

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.