Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C. Information provided provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |