MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® PC 740/4 GF20 UV WT1105-13LD PC, 20% glass fibers, UV stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled; Polycarbonate, UV Stabilized

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: Special filler, 20% glass fibers, UV stabilized

Special Features: Translucent, light scattering, high light diffusion

Market Segment: Automotive, Lighting

Application Area: Lighting, light transparent components

Typical Applications: Lamp covers, display elements, operating elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaISO 527
Elongation at Break 2.7 %ISO 527
Tensile Modulus 6000 MPaISO 527
Flexural Strength 150 MPaISO 178
Flexural Modulus 5800 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 7.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 140 °CISO 75-1/-2
Vicat Softening Point 145 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 V-2
@Thickness 0.750 mm
Glow Wire Flammability Index 850 °C
@Thickness 1.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 2.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 3.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 4.00 mm
passed; DIN EN 60695
 960 °C
@Thickness 3.00 mm
passed; DIN EN 60695
 960 °C
@Thickness 4.00 mm
passed; DIN EN 60695
 
Optical PropertiesOriginal ValueComments
Haze 95.5 %
@Thickness 1.00 mm
A,2°; ISO 13468
 95.5 %
@Thickness 2.00 mm
A,2°; ISO 13468
 95.5 %
@Thickness 3.00 mm
A,2°; ISO 13468
 95.5 %
@Thickness 4.00 mm
A,2°; ISO 13468
Transmission, Visible 21 %
@Thickness 4.00 mm
A,2°; ISO 13468
 27 %
@Thickness 3.00 mm
A,2°; ISO 13468
 37 %
@Thickness 2.00 mm
A,2°; ISO 13468
 53 %
@Thickness 1.00 mm
A,2°; ISO 13468
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °CInjection molding
Mold Temperature 80.0 - 130 °CInjection molding
Drying Temperature 120 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolycarbonate
Half Power Angle47°d=1mm, A,2°
 60°d=2mm, A,2°
 62°d=3mm, A,2°
 63°d=4mm, A,2°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® PC 740/4 UV WT1027-14LDS PC, UV stabilized
Mocom (ALBIS) ALCOM® LD PC 2020 UV 17027 WT1022-17 PC, 20% glass fibers, UV stabilized
Mocom (ALBIS) ALCOM® LD2 PC 1000 UV 17004 WT1004-17 PC
Mocom (ALBIS) ALCOM® PC 740/4 UV WT1280-04LD PC
Mocom (ALBIS) ALCOM® PC 740/4 UV WT1370-07LD PC, UV stabilized

PALBIS8150 / 242209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.