MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 9087 High Performance Double Coated Tapes with Adhesive 375
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low surface energy substrates. The excellent initial tack ensures that a bond of good integrity is achieved soon after application

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milLiner Caliper
 259 microns10.2 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.8984 kN/m5.125 pliHDPE, 180° Peel, 2-mil Al Backing; ASTM D3330
 1.3038 kN/m7.4375 pliHigh Pressure Laminate, 180° Peel, 2-mil Al Backing; ASTM D3330
 1.556 kN/m8.875 pliStainless Steel, 180° Peel, 2-mil Al Backing; ASTM D3330
 1.600 kN/m9.125 pliPolycarbonate, 180° Peel, 2-mil Al Backing; ASTM D3330
 1.600 kN/m9.125 pliABS, 180° Peel, 2-mil Al Backing; ASTM D3330
 1.797 kN/m10.25 pliGlass, 180° Peel, 2-mil Al Backing; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °FContinuous
 85.0 °C185 °FShort Term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive CarrierPVC 1.5 mils
Adhesive TypeModified Acrylic
AppearanceWhite
 White Paper (Glassine) with Green 3M Logo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33322 / 168069

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.