MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum Bronze, UNS C95300, Casting Alloy, As Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Heat treatable. Except where noted, all property values listed below are for sand casting.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Electrical applications, pickling baskets, nuts, gears, steel mill slippers, marine equipment, welding jaws, non-sparking hardware.

Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9B

Key Words: Aluminum bronze, ASTM B148, ASTM B148-9B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 1403000 kg
Hardness, Rockwell B 67
Tensile Strength, Ultimate 450 MPa
Tensile Strength, Yield 170 MPa
Elongation at Break 20 %in 50 mm
Reduction of Area 25 %
Modulus of Elasticity 110 GPa
Compressive Strength 760 MPa
Poissons Ratio 0.314
Fatigue Strength 152 MPa
@# of Cycles 1.00e+8
Machinability 55 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.0 GPa
Izod Impact 38.0 J
@Temperature -20.0 - 100 °C
Cast and annealed
Charpy Impact 31.0 J
@Temperature -20.0 - 100 °C
Keyhole, cast and annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000133 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.078 kA/m field strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 63.0 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1045 °C
Solidus 1040 °C
Liquidus 1045 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 595 - 650 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 9.0 - 11 %
Copper, Cu >= 86 %
Iron, Fe 0.80 - 1.5 %
Other, total <= 1.0 %
 
Descriptive Properties
Elastic Limit125 MPaas cast
 205 MPaTQ50 temper

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Aluminum Bronze, UNS C95200, Copper Casting Alloy
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Aluminum Bronze, UNS C95300 Casting Alloy, TQ50 Temper
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660

MC95300b1 / 11962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.