MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ THERMOTUF™ Compound QX01581H Polyamide 610 (Nylon 610)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: LNP THERMOTUF QX01581H compound is based on Nylon 6/10 resin containing 30% glass fiber. Added features of this grade include: Impact Modified.

Features: Impact Modified,Healthcare,High Stiffness,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption 0.120 - 0.200 %0.120 - 0.200 %Injection Molding
 0.200 %0.200 %23°C/50% RH/24 hrs; ASTM D570
 0.300 %0.300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/in24hrs; ASTM D955
 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 134 MPa19400 psiISO 527
 139 MPa20200 psiASTM D638
Elongation at Break 3.4 %3.4 %ASTM D638
 3.6 %3.6 %ISO 527
Tensile Modulus 7.88 GPa1140 ksi1 mm/min; ISO 527
 8.48 GPa1230 ksi50 mm/min; ASTM D638
Flexural Strength 206 MPa29900 psiASTM D790
 208 MPa30200 psiISO 178
Flexural Modulus 7.03 GPa1020 ksiASTM D790
 7.25 GPa1050 ksiISO 178
Izod Impact Notched 357 J263 ft-lbASTM D256
Izod Impact, Unnotched 11.58 J/cm21.69 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 73.0 kJ/m²34.7 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 J6.64 ft-lbpeak; ASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  30.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 32.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 208 °C
@Thickness 3.20 mm
406 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 260 - 270 °C500 - 518 °F
Zone 3 270 - 280 °C518 - 536 °F
Melt Temperature 270 - 275 °C518 - 527 °FInjection Molding
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82013 / 289960

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.