Sinpolene MBW108LE is a polyethylene-based pure white masterbatch designed specifically for use in tubular film blowing, blow molding and extrusion of polyolefins. With its high pigment loading, it offers high coloring value with excellent quality and performance. The blue undertone of this masterbatch is attributed by specially selected high performance, fine crystal size rutile titanium dioxide. It is delivered as free flowing pellets for processing convenience. Characteristic: - Easy processing
- Good dispersion
- High opacifying power
- Excellent whiteness
Availability: Asia Pacific Filler/Reinforcement: Titanium Dioxide Equivalent, 70% Filler by Weight Uses: Masterbatch; Film; Sheet RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Blown Film; Sheet Extrusion Information provided by Teknor Apex |