MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inov Chem INOVOL R6350 Polyether Polyols
Categories: Polymer

Material Notes: Introduction: The series of polyether polyols are prepared with different functionalities, hydroxyl values and viscosities based on different initiators. Mainly used in the production of polyurethane rigid foam system. Different combinations can be made according to different needs of customers for system materials to obtain different performance.

Applications: The polyurethane rigid foam system prepared by using this series of polyether polyol is mainly used for producing refrigerator freezer, pipeline insulation material, polyurethane sandwich panel, spray insulation material, wood imitation material, solar heater material, mineral material and the etc.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 5.0 - 8.05.0 - 8.0
Viscosity 4500 - 6500 cP4500 - 6500 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.50<= 0.50[mgKOH/g]
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.20 %<= 0.20 %
 
Descriptive Properties
Color=8GD
K+=20 mg/Kg
OH value480-520 mgKOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM298 / 312827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.