MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Superwool® Bulks HT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool is manufactured from pure raw materials and processed to offer excellent performance in hightemperature applications. Superwool offers an alternative to traditional solutions due to its high refractoriness and excellent non-wetting characteristics with molten aluminum. Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying. Superwool is ideally suited to individual pplications and is available in a wide range of thicknesses and densities. The maximum continuous use temperature depends on the application.

Applications:

  • Expansion Joints
  • Low Mass Kiln Cars
  • Tube Seal Fabrication
  • Thermal and Acoustical Insulation
  • Filtration Media
  • Reinforcement and Filler for Plastics, Resins and Paints
  • Fillers for Mastics, Cements and Vacuum Formed Boards and Shapes

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.08 J/g-°C
@Temperature 982 °C
0.258 BTU/lb-°F
@Temperature 1800 °F
average
Maximum Service Temperature, Air 1150 °C2100 °FContinuous Use
 
Component Elements PropertiesMetricEnglishComments
CaO+MgO 18 - 25 %18 - 25 %lime+magnesia
Other <= 3.0 %<= 3.0 %
SiO2 70 - 80 %70 - 80 %after firing
 
Descriptive Properties
Classification Temperature (°C)1300
Colorwhite
Fiber Index45-70%Grade 111
 45-70%Grade 112
 50-70%Grade HM 25
 50-70%Grade HM-50
 50-70%Grade MS-12
Fiber Length13-250 mm
 13mm
 250mm
 250mm
 25mm
 50mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Oil-Hardening Steel
FloMet 316L Stainless Steel

CMORF7069 / 203368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.