MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Precision Polymer Engineering R50Y Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Non-black, Natural Rubber, 45-55 °IRHD. Formulated to meet BS1154 Grade Y50. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber and is reinforced using zinc oxide only.

Applications: Natural rubber offers low compression set, high tensile strength, high resilience and excellent resistance to tear and abrasion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050°IRHD; ASTM D1415
Tensile Strength, Yield 15.3 MPa2220 psi-10% change after 168 hours @ 70°C; ASTM D412
 17.0 MPa2470 psiASTM D412
Elongation at Break 425 %425 %-15% change after 168 hours @ 70°C; ASTM D412
 500 %500 %ASTM D412
Compression Set 30 %
@Temperature 70.0 °C,
Time 86400 sec
30 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flash Point >= 300 °C>= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Metflex EM67 Natural Rubber
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Precision Polymer Engineering R50D Natural Rubber
Precision Polymer Engineering R50Z Natural Rubber
ATG s.r.l. NR Natural Rubber

PPRECI166 / 57890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.