MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco 100 Aviation Gasoline
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Aviation Gasolines (Avgas) 100 and 100 Low Lead are manufactured to meet the requirements of ASTM D 910, Standard Specification for Aviation Gasolines. They also may qualify for U.S. military uses, since they ASTM specification is now the basis for acceptance for such uses.

Chevron Avgas 100 is available only in Hawaii.

Applications

Chevron Avgas 100 and 100 Low Lead are intended for use in light, personal aircraft, single and twin engined executive aircraft, crop dusters, two- and four-engined transports, and certain military light aircraft which require aviation gasoline.

Piston engine aircraft are generally certified for operation on a specific grade of aviation gasoline. The use of a higher grade may be acceptable when the specified grade is not available. However, for engines designed for grade 80, continued use of Grade 100, with its higher lead content, may result in malfunctioning such as spark plug fouling. Engine manufacturer’s recommendations should be followed.

Grade 100 Low Lead is approved by most engines manufacturers for use as an alternate fuel in aircraft engines originally designed for operation on Grade 80 when it is unavailable. Engine manufacturer’s recommendations must be strictly adhered to. Check with the airframe or engine manufacturer for details.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Regular Unleaded Gasoline
Octane (CH3(CH2)6CH3)
ChevronTexaco 100 Low Lead Aviation Gasoline
ChevronTexaco Supreme Unleaded Gasoline
Unipetrol JET A-1 AFQRJOS Issue 18 Jet Kerosene

WCHEV395 / 75010

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.