MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot CAB-O-SILĀ® TS-720D Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL TS-720D fumed silica, the densed form of CAB-O-SIL TS-720 fumed silica, is a medium surface area fumed silica which has been surface modified with polydimethylsiloxane. The bulk density of CAB-O-SIL TS-720D fumed silica has been mechanically increased for faster incorporation and ease of handling.

Key applications: CAB-O-SIL TS-720D fumed silica is hydrophobic treated densed fumed silica, making it an excellent choice for moisture sensitive systems. Further, the surface chemistry of CAB-O-SIL TS-720D fumed silica makes it a very effective stable rheology control additive for medium to high polarity systems such as epoxy, urethane, and vinyl ester adhesives and bonding pastes. With its higher bulk density, CAB-O-SIL TS-720D fumed silica is faster to incorporate into formulations, but more difficult to disperse. To achieve the full performance benefits of CAB-O-SIL TS-720D fumed silica, high shear dispersion equipment is recommended. CAB-O-SIL TS-720D fumed silica is characterized by:

  • High purity
  • Aggregated structure
  • Submicron particle size
  • Low bulk density
  • Hydrophobic surface chemistry

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT102 / 315837

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.