MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Clwyd Compounders BR Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: BR Rubber is typically used in blends with other rubbers, not as a lone polymer.

Typical applications: The major use of cis polybutadiene rubber is in tires. It goes into side walls and treads to optimize performance such as traction, rolling and abrasion resistance, it is typically compounded with other elastomers such as natural rubber and SBR. Other applications are golf ball cores, inner tubes of hoses for sandblasting, and covers for pneumatic and water hoses. Polybutadiene is also used as a toughening agent in plastics, in particular in high-impact polystyrene (HIPS) andacrylonitrile-butadiene-styrene (ABS). High vinyl and high trans polybutadiene are produced on a much smaller scale and are used on amuch smaller scale. For example, high-vinly PBD is sometimes used in high quality tires to improve rebound resilience whereas high-trans PBD is used in the outer lay of golf balls.

Advantages: Butadiene rubbers are typically cured by sulfur systems and are often compounded with other polymers and additives such as oils, fillers, crosslinking agents, and antioxidants, which allows for a versatile variation of the elastomeric properties.

Disadvantages: Butadiene rubbers are not resistant to oil, gasoline and hydrocarbon solvents. They also have poor heat resistance and are susceptible to attack by ozone due to the presence of double bonds in the polymer backbone which are prone to thermal-oxidative degradation. The degradation generally occurs through oxidative crosslinking and causes embrittlement.

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 9040 - 90
Tensile Strength <= 20.0 MPa<= 2900 psi
Elongation at Break <= 550 %<= 550 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FUpper continuous
Minimum Service Temperature, Air -90.0 °C-130 °Fnon-brittle
 -60.0 °C-76.0 °Fsealing applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCLWYD027 / 316044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.