MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller 145 Pipe, Fitting and Thread Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 145 is a liquid sealant for locking and sealing high pressure fluid power systems and will not clog filters.

Features and Benefits:

  • High Pressure Fluid Sealant
  • No Filter Contamination
  • Controlled Flow Viscosity

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Brookfield Viscosity 10000 cP10000 cPSpindle 3, 20 rpm
Storage Temperature 8.00 - 28.0 °C46.4 - 82.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.100 µm/m-°C0.0556 µin/in-°FASTM D696
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flash Point >= 93.0 °C>= 199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorPurple
ConsistencyLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL172 / 316963

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.