MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BigRep PA6/66 Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: It is a light-weight thermoplastic material with high rigidity, and has high resistance to heat and chemicals. Its high compatibility with machining and mechanical strength make it an excellent candidate for most industrial applications, especially in the automotive and aerospace sectors.Functionally similar to Nylon PA6, a common material for injection molding, PA6/66 is ideal for printing end-use parts or prototyping with nearly identical material properties to final, mass produced parts. The material's durability and production scalability make it the choice for not just industrial transportation applications, but also developing product electrical housing, cooling and heating systems, as well as molds and vacuum forming.Prototyping with PA6/66 in full-scale with the same material properties as a final product can present substantial shortcuts in the product development cycle, circumventing frequent late stage iteration problems and dodging related exorbitant expenses.

TPU AT A GLANCE:

  • Heat Resistance up to 180° C
  • Chemical Resistance
  • High Mechanical Strength
  • Low-Weight Products
  • Easily Machined

Information provided by Bigrep

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Filament Diameter 2850 µm2850 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 67.0 MPa9720 psiISO 527
Elongation at Break 10 %10 %ISO 527
Tensile Modulus 2.325 GPa337.2 ksiYoung’s; ISO 527
Flexural Strength 98.0 MPa14200 psiISO 178
Flexural Modulus 1.725 GPa250.2 ksiISO 178
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 190 °C374 °F
Vicat Softening Point 180 °C356 °FISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 250 - 270 °C482 - 518 °F
 
Descriptive Properties
Environmental temperature40 - 60 °C
Filament Net Weight3.0, 4.5, 8.0 kg
Heating Bed0-75°C
Printing Speed>40 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIGR005 / 250855

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.