MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
GEHR Plastics POM-ESD-FG Polyoxymethylene
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Variant of POM (Copolymer) with an improved electrical conductivity. Surface resistivity =1011 O. Polyoxymethylene can be used in temperatures ranging from -58 °F to +230 °F. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and good resistance to wear because of the high strength and smooth surface. There is a very low risk of stress cracks.

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %ISO 62
Water Absorption at Saturation 0.80 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868
Tensile Strength at Break 54.0 MPaISO 527
Tensile Strength, Yield >= 56.0 MPaISO 527
Elongation at Break 25 %ISO 527
Elongation at Yield 20 %ISO 527
Modulus of Elasticity 2.67 GPaISO 527
Charpy Impact Unnotched 180 kJ/m²ISO 179
Charpy Impact, Notched 6.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+10 ohm-cmIEC 60093
Surface Resistance <= 1.00e+12 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°CISO 11359
Melting Point 168 °CISO 3146
Maximum Service Temperature, Air 100 °CUL 746B
Glass Transition Temp, Tg -60.0 °CISO 3146
Flammability, UL94 HBtest results without UL registration; UL 94
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Acid ResistanceYes
Aromatic ResistanceYes
CKW ResistanceLimited
Hydrocarbonate ResistanceYes
Hydroxide ResistanceYes
Ketone ResistanceYes
Physiological indifferenceyes, EEC
Resistance to Hot WaterYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company ESD 303 EM Polycarbonate (PC), Glass Fiber - ESD Protection - Static Dissipative - Easy Molding
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
Aluminum, Al
Ensinger Delrin® 150 Homopolymer Acetal (POM)

PGEHR027c / 122035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.