MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium WE54-T6, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Nd content refers to Nd-rich rare earths.

Key Words: UNS M18410; Aerospace Alloy; Mg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 85500 kg load, 10 mm ball
Hardness, Knoop 109Estimated from Brinell
Hardness, Rockwell A 36Estimated from Brinell
Hardness, Rockwell B 53Estimated from Brinell
Hardness, Vickers 96Estimated from Brinell
Tensile Strength, Ultimate 280 MPa
Tensile Strength, Yield 225 MPa
@Strain 0.2 %
Elongation at Break 4.0 %in 50 mm
Tensile Modulus 44.4 GPa
Compressive Yield Strength 172 MPaat 0.2% offset
Poissons Ratio 0.27
Shear Modulus 17.0 GPaEstimated from similar Mg alloys.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000173 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 370 J/gEstimated from trends in similar Mg alloys.
CTE, linear 26.0 µm/m-°C
@Temperature 0.000 - 100 °C
Estimated from similar Mg alloys.
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°CTypical Mg alloy value.
Thermal Conductivity 52.0 W/m-K
Melting Point 550 - 640 °C
Solidus 550 °C
Liquidus 640 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 750 - 820 °CSand Casting
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.030 %
Lithium, Li <= 0.20 %
Magnesium, Mg 91 %As Remainder
Manganese, Mn <= 0.15 %
Neodymium, Nd 2.0 - 4.0 %Nd-rich rare earths
Nickel, Ni <= 0.0050 %
Silicon, Si <= 0.010 %
Yttrium, Y 4.75 - 5.5 %
Zinc, Zn <= 0.20 %
Zirconium, Zr 0.40 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
Magnesium Elektron Elektron® WE54 Magnesium Casting Alloy, UNS M18410
Magnesium WE43-T6, Cast
Magnesium EA65RS-T4, Extruded
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311

MMWE54 / 12464

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.