Chemical Name: Barium stearate CAS No.: 6865-35-6 Molecular Fomula: C36H70BaO4 Description: Barium stearate is white fine powder, insoluble in water. When mixed with hot, strong mineral acids, they decomposed into stearic acid and corresponding barium salts. This series product has good thermo stability and processing performance, reasonable formulation. It has excellent internal and external Iubricating balance; do not need any more Iubricant. It 15 especially suitable for pressure pipes, has wide compatibility to the different feed rate and different quality padding. Application: Used as machine high temperature resistant lubricants, rubber products of high temperature resistant additives, PVC plastic light heat stabilizer. the thermal stability of PVC products agent.a waterproofing agent, lubricant and bearing lining. high-temperature resistant powder for rubber products. It can be Used as PVC stabilizer and lubricant. In all of the alkaline earth metal stearate, it has the best heat-resistance. It is mainly used for transparent film, sheet, artificial leather and soft plate, pipe, etc. It also can be used as high- temperature stripping agent and mechanical with high temperature lubricant. heat stabilizer of vinyl chloride copolymer. It has good long-term heat resistance and lubricity, stable effect than calcium stearate, but less than lead stearate. Information provided by Konson® |