MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Formosa Plastics Formolene® HB5502F Blow Molding HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: High Density Polyethylene Hexene Copolymer with Synthetic Antistat

Formolene® HB5502F HDPE resin is designed for applications requiring excellent stiffness and stress crack resistance properties. It may be used as a blow molding resin or sheet extrusion thermoforming resin.

Formolene® HB5502F meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Applications: Blow molding – Pharmaceuticals, Food Packaging, Industrial Chemicals and Industrial Parts; Molding or Forming - Industrial Parts and Pallets

Physical properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928.

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D1505
ESCR 100% Igepal® 30 hour30 hourCondition B, F50; ASTM D1693
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.6 MPa4000 psi2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 600 %>= 600 %2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 1.03 GPa150 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -84.0 °C<= -119 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese GUR® 2122 PE-UHMW, Specialty
Special Metals NILO® Alloy 36 Low-Expansion Alloy
Entec Hypel® PEHD18/.956 HDPE
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE)
Chevron Phillips Marlex® 9514H Polyethylene; HDPE

PFPCPQ044 / 150276

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.