MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eneos N220S Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics: Typical High AN NBR

Application: Various packings, gaskets, hoses, PVC blends, adhesives

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Mooney Viscosity  41
@Temperature 100 °C
41
@Temperature 212 °F
ML1+4
 62
@Temperature 100 °C
62
@Temperature 212 °F
ML1+4, Compound (non-vulcanized)
 36
@Temperature 125 °C,
Time 64800 sec
36
@Temperature 257 °F,
Time 18.0 hour
Scorch Test, ML1, Compound (non-vulcanized)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272
 7272Compound (vulcanized)
 58
@Temperature 40.0 °C,
Time 173000 sec
58
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
 65
@Temperature 120 °C,
Time 252000 sec
65
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
 70
@Temperature 120 °C,
Time 252000 sec
70
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
 78
@Temperature 120 °C,
Time 252000 sec
78
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
Tensile Strength 22.7 MPa3290 psi
 22.7 MPa3290 psiCompound (vulcanized)
 14.301 MPa
@Temperature 40.0 °C,
Time 173000 sec
2074.2 psi
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
 19.976 MPa
@Temperature 120 °C,
Time 252000 sec
2897.3 psi
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
 22.7 MPa
@Temperature 120 °C,
Time 252000 sec
3290 psi
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
 23.835 MPa
@Temperature 120 °C,
Time 252000 sec
3457.0 psi
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
Elongation at Break 470 %470 %
 470 %470 %Compound (vulcanized)
 282 %
@Temperature 120 °C,
Time 252000 sec
282 %
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
 286.7 %
@Temperature 120 °C,
Time 252000 sec
286.7 %
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
 296.1 %
@Temperature 40.0 °C,
Time 173000 sec
296.1 %
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
 68479 %
@Temperature 120 °C,
Time 252000 sec
68479 %
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
100% Modulus 3.70 MPa537 psiCompound (vulcanized)
300% Modulus 17.3 MPa2510 psi
 17.3 MPa2510 psiCompound (vulcanized)
Resilience 1818[%], Rebound, Compound (vulcanized)
Tear Strength 53.0 kN/m302 pliCompound (vulcanized)
Compression Set  13 %
@Temperature 100 °C,
Time 252000 sec
13 %
@Temperature 212 °F,
Time 70.0 hour
Compound (vulcanized)
 19 %
@Temperature 120 °C,
Time 252000 sec
19 %
@Temperature 248 °F,
Time 70.0 hour
Compound (vulcanized)
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -18.0 °C-0.400 °F
 
Descriptive Properties
Acrylonitrile Content (%)41
Delta;V100 (%)2Distilled Water 70 hr at 40°C, Compound (non-vulcanized)
 -2IRM901 70 hrs at 120°C, Compound (vulcanized)
 20Fuel Oil B 48 hrs at 40°C, Compound (non-vulcanized)
 34Fuel Oil C 48 hrs at 40°C, Compound (non-vulcanized)
 59Fuel Oil C/Ethanol 48 hrs at 40°C, Compound (non-vulcanized)
 8IRM903 70 hrs at 120°C, Compound (vulcanized)
Extrusion Test11080°C, 25 rpm, Die Swell %
 407 cm/min80°C, 25 rpm, Extrusion Length
 428 cc/min80°C, 25 rpm, Extrusion Volume
Flex Test20Occurrence(Thousand Times)
 4Growth 2 to 15 mm (Thousand Times)
Flow Rate115Q×104, 80°C, 100 kg, Kokahiki Flow tester
JSR Mold Curast Test 160°C, Minutes2tc(10)
 6tc(90)
Low-Temperature Torsion Test-15°Ct10
 -23°Ct100
Mill Contraction 50°C (%)34
Ozone Degradability TestC-3Static 20% Elongation, 50 ppm 5 Hours at 40°C
 C-3Dynamic 0 to 20% Elongation, 50 ppm 5 Hours at 40°C
Product formBale
Product StainNS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8051 / 295367

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.