MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Insulcast® 3316 HFR-S Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 3316 HFR-S is a fast setting, low viscosity, flame-retardant (V-0) epoxy system designed for casting applications. When cured with INSULCURE 383 Blue, it gives room temperature cures in 12 hours. This system combines the features of several systems. It has excellent thermal conductivity, very high peel strength, good thermal shock resistance and a smooth glossy surface upon cure. INSULCAST 3316 HFR-S can also be used as an adhesive system, setting in thin films in about 2 hours.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccuncured. Insulcure 383 Blue
 1.80 g/cc1.80 g/ccuncured
Viscosity 500 cP500 cPInsulcure 383 Blue; ASTM D2393
 24000 cP24000 cPmixed
 24000 cP24000 cPmixed. Insulcure 383 Blue
 30000 cP30000 cPuncured; ASTM D2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 9080 - 90ASTM D2240
Tensile Strength 29.0 MPa4200 psiASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm400 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Gel Time 10.0 - 15.0 min10.0 - 15.0 minInsulcure 383 Blue
 10.0 - 15.0 min
@Temperature 25.0 °C
10.0 - 15.0 min
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 MonthInsulcure 383 Blue.
 12.0 Month12.0 Month
 
Descriptive Properties
ColorblueUncured. Insulcure 383 Blue
 whiteUncured. Insulcast
Mix Ratio by weight100:20-253316 HFR-S:Insulcure 383 Blue
Thermal Shock-55 to 100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9091 / 239601

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.