MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ FG171 Polyamide 66, GF Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccDry as Molded; ASTM D792
Density 1.54 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 0.80 %
@Temperature 23.0 °C
50% RH; ISO 62
 0.80 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55Conditioned at 50% RH; ISO 2039
 95Dry as Molded; ISO 2039
Tensile Strength at Break 121 MPaDry as Molded; ISO 527
 154 MPaConditioned at 50% RH; ISO 527
Tensile Strength 127 MPaConditioned at 50% RH; ASTM D638
 162 MPaDry as Molded; ASTM D638
Elongation at Break 2.5 %Dry as Molded; ISO 527
 3.0 %Conditioned at 50% RH; ISO 527
Tensile Modulus 8200 MPaConditioned at 50% RH; ISO 527
 10200 MPaDry as Molded; ISO 527
Flexural Strength 180 MPaConditioned at 50% RH; ISO 178
 244 MPaDry as Molded; ISO 178
Flexural Modulus 7900 MPaConditioned at 50% RH; ISO 178
 9700 MPaDry as Molded; ISO 178
Izod Impact, Notched 92.0 J/mDry as Molded; ASTM D256
 110 J/mConditioned at 50% RH; ASTM D256
Charpy Impact Unnotched 67.0 kJ/m²Conditioned at 50% RH; ISO 179
 67.0 kJ/m²Dry as Molded; ISO 179
Charpy Impact, Notched 11.0 kJ/m²Dry as Molded; ISO 179
 12.0 kJ/m²Conditioned at 50% RH; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDry as Molded; IEC 60093
Surface Resistance 1.00e+14 ohmDry as Molded; IEC 60093
Dielectric Strength 28.0 kV/mmDry as Molded; IEC 60243
Comparative Tracking Index 275 V
@Thickness 3.00 mm
Dry as Molded; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CDry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi) 256 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 240 °CDry as Molded; ISO 75
Flammability, UL94 V-0
@Thickness 0.750 mm
Dry as Molded
Glow Wire Flammability Index 960 °CDry as Molded; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASAHI8164 / 221191

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.