MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Morsil ™ Nitride Bonded Silicon Carbide
Categories: Ceramic; Carbide; Nitride

Material Notes: Bond type: Silicon Nitride.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.68 g/cc0.0968 lb/in³ASTM C134
Porosity 17 %17 %
Permeability 3.03.0(cc of air/min/in/m2/in WG press)
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0430 GPa
@Temperature 20.0 °C
6.24 ksi
@Temperature 68.0 °F
 0.0440 GPa
@Temperature 1350 °C
6.38 ksi
@Temperature 2460 °F
Compressive Strength 37.0 MPa5370 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.46 µm/m-°C4.70 µin/in-°F
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 16.3 W/m-K
@Temperature 1204 °C
113 BTU-in/hr-ft²-°F
@Temperature 2199 °F
ASTM C 202
Maximum Service Temperature, Air 1760 °C3200 °FMax hot face temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.30 %0.30 %
CaO 0.20 %0.20 %
Fe2O3 0.30 %0.30 %
Other 0.30 %0.30 %trace
Si3N4 23.4 %23.4 %
SiC 75 %75 %
SiO2 0.50 %0.50 %
 
Descriptive Properties
Electrical Characteristicssemi-conductor
Hot Load Contractions (% of length)0
Spall Resistance (%)100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Aluminum 99/Silicon 1 Alloy
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Alpase M-5™ Aluminum Mold Plate
Arkema Kynar Flex® 2801-00 Polyvinylidene Fluoride Powder
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide

CMORF6088 / 202872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.