MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C51900, OS025 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.025 mm

Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Spot Weld; Fair Suitability – Oxyacetylene Welding; Poor Suitability – Coated Metal Arc Welding, Seam Weld, Capacity for Being Hot Formed

Typical Uses: Electrical Connectors; Electrical Flexing Contact Blades; Electronic Connectors

Applicable Specifications: Bar – ASTM B103/B103M; Plate - ASTM B103/B103M; Sheet - ASTM B103/B103M; Strip - ASTM B103/B103M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 365 MPa53000 psi
Tensile Strength, Yield 193 MPa28000 psi0.2% Offset
Elongation at Break 56 %56 %
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000123 ohm-cm0.0000123 ohm-cm14% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 100 °C
10.0 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 5.48 W/m-K38.0 BTU-in/hr-ft²-°F
Melting Point 927 - 1040 °C1700 - 1900 °F
Solidus 927 °C1700 °F
Liquidus 1040 °C1900 °F
Annealing Point 21.1 - 732 °C70.0 - 1350 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 92.2 - 95 %92.2 - 95 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P 0.030 - 0.35 %0.030 - 0.35 %
Tin, Sn 5.0 - 7.0 %5.0 - 7.0 %
Zinc, Zn <= 0.30 %<= 0.30 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC51900y2 / 292150

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.