MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:
  • Engineered for excellent mechanical properties, part definition and surface finish.
  • Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates from 15 to 25%.
  • Good temperature control is required to process this material.

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.420 g/cc0.0152 lb/in³ASTM D1895
Density 0.870 g/cc0.0314 lb/in³Sintered; ASTM D792
Particle Size 50 µm50 µmD50
 38 - 78 µm38 - 78 µmD10-D90
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 235 °C
13 g/10 min
@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 37.0 MPa5370 psiZ; ASTM D638
 48.0 MPa6960 psiXY; ASTM D638
Elongation at Break 3.0 %3.0 %Z; ASTM D638
 4.0 %4.0 %XY; ASTM D638
Tensile Modulus 2.137 GPa309.9 ksiZ; ASTM D638
 3.378 GPa489.9 ksiXY; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Avient Therma-Tech™ NJC-7500 Nylon 12
Avient Therma-Tech™ NJC-6500 Nylon 12
Ashley Polymers Ashlene® TD930H Nylon 12
Avient Therma-Tech™ NJC-8500 Nylon 12

PALP88 / 177149

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.