MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Tefzel™ ETFE HT-2188 Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Tefzel™ ETFE HT-2188 is a special purpose fluoroplastic resin available in translucent, 2.5-mm (0.1-in) pellets. Compared with other grades of Tefzel™ , it has a higher flow rate, low melting point, and high flexural endurance. Tefzel™ ETFE HT-2188 and the other Tefzel™ fluoroplastics are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. Tefzel™ ETFE HT-2188 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, such as tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Bulk Density 1.30 g/cc0.0470 lb/in³Chemours Test
Water Absorption 0.0070 %
@Time 86400 sec
0.0070 %
@Time 24.0 hour
ASTM D270
Melt Flow 15 g/10 min15 g/10 minASTM D3159
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 250 %250 %ASTM D1457
Elongation, Ultimate 300 %300 %ASTM D638
Flexural Modulus 0.860 GPa125 ksiASTM D790
Compressive Strength 38.0 MPa5510 psiASTM D695
Flex Crack Resistance 10000 - 2700010000 - 27000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBNBASTM D256
Coefficient of Friction 0.030 - 0.400.030 - 0.40ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm
@Frequency 1e+6 Hz
1.00e+15 ohm-cm
@Frequency 1e+6 Hz
ASTM D257
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 2.5 - 2.6
@Frequency 1e+6 Hz
2.5 - 2.6
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 70.0 kV/mm
@Thickness 0.250 mm
1780 kV/in
@Thickness 0.00984 in
ASTM D150
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
ASTM D1531
Arc Resistance 122 sec122 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 126 µm/m-°C
@Temperature 0.000 - 100 °C
70.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Melting Point 230 °C446 °FASTM D3418
Maximum Service Temperature, Air 150 °C302 °FUL 746
Flammability, UL94 V-0V-0
Oxygen Index 30 - 32 %30 - 32 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Heat of Combustion13.7 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceExcellent
Weather Resistance (years unaffected)15Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8780 / 268706

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.