MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hybrid Plastics Fireban® Mark VII Resorcinolinic (PRF)
Categories: Polymer

Material Notes: The resin system produces a superiour fire resistant material.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccresin age: 0-3 months
 1.24 g/cc1.24 g/ccresin age: 6 months
Solids Content 76 %76 %
pH  7.78
@Temperature 25.0 °C
7.78
@Temperature 77.0 °F
resin age: 0-3 months
 7.78
@Temperature 25.0 °C
7.78
@Temperature 77.0 °F
resin age: 6 months
Brookfield Viscosity 1500 - 2000 cP1500 - 2000 cPresin age: 0-3 months
 2700 - 3000 cP2700 - 3000 cPresin age: 6 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 55 - 7555 - 75
Tensile Strength, Ultimate >= 150 MPa>= 21800 psi
Flexural Strength >= 250 MPa>= 36300 psi
Compressive Strength >= 190 MPa>= 27600 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56resin age: 0-3 months
 1.561.56resin age: 6 months

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHYBR020 / 78830

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.