MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Chemical Cilbond® 24 Bonding Agent
Categories: Other Engineering Material

Material Notes: Cilbond 24 is a one-component bonding system developed to give high performance bonding with the following elastomers:
  • Natural Rubber (NR)
  • Polychloroprene Rubber (CR)
  • Synthetic Poyisoprene Rubber (IR)
  • Polyacrylate (ACM)
  • Ethylene Acrylate/Vamac® C (AEM)
  • Styrene Butadine Rubber (SBR)
  • Polybutadiene (BR)
  • Polyepichlorohydrin (ECO)
  • Chlorosulphonated Polyethylene (CSM/ACSM)
  • Carboxylated NBR (XNBR)
  • Polynorbornene
  • Ethylene Vinyl Acetate EVA (EVM)
Cilbond 24 has also been designed as an effective post-vulcanizing (PV) bonding system and has the further benefit of being suitable for bonding rubbers to certain fibers, cords and fabrics, such as cellulose, polyamides, polyester and glass.

Information provided by HB Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Solids Content 18.5 %18.5 %
Volatiles 75 %75 %
Viscosity Measurement 17
@Temperature 25.6 °C
17
@Temperature 78.0 °F
[sec], No 3 Zahn Cup
 
Thermal PropertiesMetricEnglishComments
Flash Point -32.8 °C-27.0 °FAbel Pensky
 -30.6 °C-23.0 °FSeta Flash
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlack Liquid
Bonding Temperature250-445°F
Content0.31HAP
Typical Coverage610 ft2/US galat 15 microns/0.6 mil (dry)
VOC0.75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBCHEM025 / 317444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.