MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik NiCu30Fe Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Sandvik NiCu30Fe is a nickel-copper (NiCu) based alloy with very good corrosion resistance to several media containing chlorides and alkalis and acid environments such as sulphuric, hydrochloric and hydrofluoric acids. The grade has good mechanical and fabrication properties. Sandvik NiCu30Fe is recommended for use under certain conditions in, for example, sea water or in the manufacture of special sealing joints for the petrochemical industry. Since this alloy has a low carbon content, it facilitates cold fabrication and is being largely applied in the production of eyeglass frames and electric/electronic components.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Copper, Cu 32.5 %
Iron, Fe 1.45 %
Nickel, Ni 66.02 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5216 / 199780

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.